  • Physical Characteristics

    Metal contentFe: 5.90 – 6.10 %
    Non-volatile content43.00 – 53.00 % ASTM D 1644
    ViscosityA-5 to K ASTM D 2373 (25 °C)
    Specific gravity0.900 – 0.940 (25°C) ASTM D 1963
    Weight per gallon7.50 – 7.83 lb/gal ASTM D 1963

  • Features

    • Primary drier
    • Improves through-drying
    • Develops full effect at high temperatures (> 150 °C)
    • Rapid surface drying
    • Acts as an adhesion promoter in anti-corrosion coatings

  • Applications

    • Coatings which dry by oxidation and are stoved at high temperatures, including:
      • Oil-based baking systems for cans
      • Dark-colored baking systems
    • Anti-corrosion coatings

  • Dosage

    In our experience, the percentage addition of iron, calculated on the metal content per binder (solid), is approx. 0.1 – 1.0 % Fe. The exact amount required depends on the binder used.

  • Storage

    Protect from the effects of weathering and store at temperatures below 50 °C. Once opened, containers should be resealed immediately after each removal of the product.

  • Safety

    Please refer to our safety data sheet for information relating to product safety.

Registration :

For chemical inventory status, please review section 15 of the current SDS.

Click here to access the SDS portal.

For additional regulatory information, please contact [email protected].